Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 2.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3660T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.10 MPa

@Strain 300 %
305 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3838 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.10 MPa

@Strain 200 %
305 psi

@Strain 200 %
ASTM D412
Teknor Apex Monprene® MP-2815A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 2.10 MPa

@Strain 300 %
305 psi

@Strain 300 %
ASTM D412
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer
Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i..
Tensile Stress 2.10 MPa

@Strain 300 %
305 psi

@Strain 300 %
ASTM D412
ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film
Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced us..
Tensile Stress 2.10 MPa

@Strain 0.160 %,
Temperature 180 °C
305 psi

@Strain 0.160 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per..
Tensile Stress 2.10 MPa

@Strain 10.0 %
305 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EL250 TPC-ET
Injection Molding
Tensile Stress 2.10 MPa

@Strain 10.0 %
305 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8351 NC021 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D Easy-to-Strip UV Stabilized Polyester Elastomer with Non-discoloring Stabilizer Developed for Extrusion Information provided by DuPont Performance Polymers
Tensile Stress 2.10 MPa

@Strain 5.00 %
305 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients..
Tensile Stress 2.10 MPa

@Strain 5.00 %
305 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers
Tensile Stress 2.10 MPa

@Strain 300 %
305 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P55A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P55A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.10 MPa

@Strain 300 %
305 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P55A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P55A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..