Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.50 MPa @Strain 300 % |
363 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 2.50 MPa @Strain 300 %, Temperature 23.0 °C |
363 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Tensile Stress | 2.50 MPa @Strain 50.0 % |
363 psi @Strain 50.0 % |
Average; ASTM D412 Method A |
Seals Eastern 7040 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Stress | 2.50 MPa @Strain 0.0500 %, Temperature -20.0 °C |
363 psi @Strain 0.0500 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 2.50 MPa @Strain 0.830 %, Time 3.60e+6 sec |
363 psi @Strain 0.830 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Tensile Stress | 2.50 MPa @Strain 10.0 %, Temperature 23.0 °C |
363 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
Tensile Stress | 2.50 MPa @Strain 5.00 % |
363 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 2.50 MPa @Strain 5.00 % |
363 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G4078 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.50 MPa @Strain 5.00 %, Temperature 23.0 °C |
363 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | >= 2.50 MPa @Strain 100 % |
>= 363 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 270A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 2.50 MPa @Strain 300 % |
>= 363 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 365A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | >= 2.50 MPa @Strain 100 % |
>= 363 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 2.50 MPa @Strain 300 % |
>= 363 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 765A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Stress | >= 2.50 MPa @Strain 100 % |
>= 363 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 770A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Stress | 2.50 MPa @Strain 300 % |
363 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G45A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.50 MPa @Strain 300 % |
363 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G45A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G45A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.50 MPa @Strain 10.0 % |
363 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |