Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 363 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.50 MPa

@Strain 300 %
363 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 2.50 MPa

@Strain 300 %,
Temperature 23.0 °C
363 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Tensile Stress 2.50 MPa

@Strain 50.0 %
363 psi

@Strain 50.0 %
Average; ASTM D412 Method A
Seals Eastern 7040 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Stress 2.50 MPa

@Strain 0.0500 %,
Temperature -20.0 °C
363 psi

@Strain 0.0500 %,
Temperature -4.00 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 2.50 MPa

@Strain 0.830 %,
Time 3.60e+6 sec
363 psi

@Strain 0.830 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
Tensile Stress 2.50 MPa

@Strain 10.0 %,
Temperature 23.0 °C
363 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® G3548L TPC-ET  (Unverified Data**)
Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec..
Tensile Stress 2.50 MPa

@Strain 5.00 %
363 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 2.50 MPa

@Strain 5.00 %
363 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G4078 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 2.50 MPa

@Strain 5.00 %,
Temperature 23.0 °C
363 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Tensile Stress 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress >= 2.50 MPa

@Strain 100 %
>= 363 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 270A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 2.50 MPa

@Strain 300 %
>= 363 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 365A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 2.50 MPa

@Strain 100 %
>= 363 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 2.50 MPa

@Strain 300 %
>= 363 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 765A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress >= 2.50 MPa

@Strain 100 %
>= 363 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 770A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress 2.50 MPa

@Strain 300 %
363 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G45A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.50 MPa

@Strain 300 %
363 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G45A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G45A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.50 MPa

@Strain 10.0 %
363 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved