Polymer Property : Tensile Stress = 2216 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 15.28 MPa

@Strain 1.77 %,
Temperature 150 °C
2216 psi

@Strain 1.77 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Tensile Stress 15.28 MPa

@Strain 0.400 %,
Temperature 150 °C
2216 psi

@Strain 0.400 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It..