Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 13.0 - 17.0 MPa

@Strain 100 %
1890 - 2470 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Stress 13.0 - 17.0 MPa

@Strain 100 %
1890 - 2470 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..