Polymer Property : Tensile Stress = 1890 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 13.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
1890 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET  (Unverified Data**)
Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In..
Tensile Stress 13.0 MPa

@Strain 10.0 %,
Temperature 150 °C
1890 psi

@Strain 10.0 %,
Temperature 302 °F
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 13.0 MPa

@Strain 10.0 %
1890 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 13.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1890 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 13.0 MPa

@Strain 100 %
1890 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 13.0 MPa

@Strain 100 %
1890 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 13.0 MPa

@Strain 0.550 %,
Temperature 0.000 °C
1890 psi

@Strain 0.550 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided..
Tensile Stress 13.0 MPa

@Strain 100 %
1890 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer
Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 13.0 MPa

@Strain 300 %
1890 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 13.0 - 17.0 MPa

@Strain 100 %
1890 - 2470 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Stress 13.0 - 17.0 MPa

@Strain 100 %
1890 - 2470 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..