Material Notes:
OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to typical OnFlex™-S properties such as a wide hardness range, good mechanical properties, good processability, good colourability and a wide temperature operating range. OnFlex™-S EH compounds are filled, and are therefore opaque and have a moderately high density.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength at Break 5.00 MPa
725 psi
ISO 37
Tensile Stress 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 37
3.20 MPa

@Strain 300 %
464 psi

@Strain 300 %
ISO 37
Elongation at Break 550 %
550 %
ISO 37
Tear Strength 26.0 kN/m
148 pli
ISO 34-1
Compression Set 29 %

@Temperature 23.0 °C,
Time 259000 sec
29 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
50 %

@Temperature 70.0 °C,
Time 79200 sec
50 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
78 %

@Temperature 100 °C,
Time 79200 sec
78 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Descriptive Properties Value Comments
Features General Purpose
Fogging 1.2 mg
DIN 75201B; 100°C
Forms Pellets
Generic Material TPE
Generic Material Type Styrenic Thermoplastic Elastomer (TES)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Fast
Manufacturer / Supplier GLS Thermoplastic Elastomers
Odor rating 2.4
VDA 270
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliances
Automotive Applications
Consumer Applications
General Purpose
Industrial Applications