Mechanical Properties Metric English Comments
Tensile Stress 3.00 MPa

@Strain 100 %
435 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 3.00 MPa

@Strain 100 %
435 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S KE 70A-3S1726 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
Tensile Stress 3.00 MPa

@Strain 100 %
435 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Stress 3.00 MPa

@Strain 100 %,
Temperature 23.0 °C
435 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
Tensile Stress 3.00 MPa

@Strain 100 %
435 psi

@Strain 100 %
Average; ASTM D412 Method A
Seals Eastern 5753 Fluorocarbon-Elastomer
Features:MIL-SpecFKM general serviceInformation provided by Seals Eastern.
Tensile Stress 3.00 MPa

@Strain 0.0960 %,
Time 3600 sec
435 psi

@Strain 0.0960 %,
Time 1.00 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Tensile Stress 3.00 MPa

@Strain 0.103 %,
Time 36000 sec
435 psi

@Strain 0.103 %,
Time 10.0 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Tensile Stress 3.00 MPa

@Strain 0.111 %,
Time 360000 sec
435 psi

@Strain 0.111 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Tensile Stress 3.00 MPa

@Strain 0.121 %,
Time 3.60e+6 sec
435 psi

@Strain 0.121 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Tensile Stress 3.00 MPa

@Strain 0.130 %,
Time 3.60e+7 sec
435 psi

@Strain 0.130 %,
Time 10000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Tensile Stress 3.00 MPa

@Strain 10.0 %
435 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® XG5855 TPC-ET
Extrusion Grade
Tensile Stress 3.00 MPa

@Strain 5.00 %,
Temperature 23.0 °C
435 psi

@Strain 5.00 %,
Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Tensile Stress 3.00 MPa

@Strain 0.165 %,
Time 36000 sec
435 psi

@Strain 0.165 %,
Time 10.0 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Tensile Stress 3.00 MPa

@Strain 0.192 %,
Time 360000 sec
435 psi

@Strain 0.192 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Tensile Stress 3.00 MPa

@Strain 0.231 %,
Time 3.60e+6 sec
435 psi

@Strain 0.231 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Tensile Stress 3.00 MPa

@Strain 0.146 %,
Time 3600 sec
435 psi

@Strain 0.146 %,
Time 1.00 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Tensile Stress 3.00 MPa

@Strain 0.297 %,
Time 3.60e+7 sec
435 psi

@Strain 0.297 %,
Time 10000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Tensile Stress 3.00 MPa

@Strain 300 %
435 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G55A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G55A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.00 MPa

@Strain 100 %
435 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer
Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 3.00 MPa

@Strain 300 %
>= 435 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 265A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 3.00 MPa

@Strain 100 %
>= 435 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 465A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 3.00 MPa

@Strain 300 %
435 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G55A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G55A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Copyright © lookpolymers.com All Rights Reserved