Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Austin Novel Materials Texalan® 265A Polyester-based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 265A Polyester-based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 62 - 68
62 - 68
ISO 7619
Tensile Strength >= 18.0 MPa
>= 2610 psi
ISO 37
Tensile Stress >= 1.50 MPa

@Strain 100 %
>= 218 psi

@Strain 100 %
ISO 37
>= 3.00 MPa

@Strain 300 %
>= 435 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 850 %
>= 850 %
ISO 37
Tear Strength >= 45.0 kN/m
>= 257 pli
ISO 34
K Factor (Wear Factor) <= 70
<= 70
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 30 %

@Temperature 70.0 °C
<= 30 %

@Temperature 158 °F
ISO 815
Users viewing this material also viewed the following: