Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.20 MPa @Strain 300 % |
464 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S EH 70A-3S7004 Thermoplastic Elastomer (TPE) OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Stress | 3.20 MPa @Strain 300 % |
464 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3653T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.20 MPa @Strain 100 % |
464 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3870 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.20 MPa @Strain 10.0 %, Temperature 23.0 °C |
464 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
Tensile Stress | 3.20 MPa @Strain 10.0 % |
464 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.20 MPa @Strain 10.0 % |
464 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.20 MPa @Strain 300 % |
464 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G60A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G60A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.20 MPa @Strain 300 % |
464 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G60A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G60A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |