Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 65.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 65.0 MPa

@Strain 4.00 %,
Temperature 120 °C
9430 psi

@Strain 4.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 65.0 MPa

@Strain 8.00 %,
Temperature 150 °C
9430 psi

@Strain 8.00 %,
Temperature 302 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 65.0 MPa

@Strain 2.00 %,
Temperature 120 °C
9430 psi

@Strain 2.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 65.0 MPa

@Strain 1.00 %,
Temperature 23.0 °C
9430 psi

@Strain 1.00 %,
Temperature 73.4 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 65.0 MPa

@Strain 2.00 %,
Temperature 150 °C
9430 psi

@Strain 2.00 %,
Temperature 302 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 65.0 MPa

@Strain 10.9 %,
Temperature 23.0 °C
9430 psi

@Strain 10.9 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..
Tensile Stress 65.0 MPa

@Strain 4.00 %,
Temperature 40.0 °C
9430 psi

@Strain 4.00 %,
Temperature 104 °F
ISO 527
BASF Ultradur B 4300 G2 10% Glass Filled PBT
Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..