Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.20 MPa @Strain 300 % |
1190 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4885 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 8.20 MPa @Strain 1.10 %, Temperature 90.0 °C |
1190 psi @Strain 1.10 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 8.20 MPa @Strain 15.0 %, Temperature 23.0 °C |
1190 psi @Strain 15.0 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
Tensile Stress | 8.20 MPa @Strain 157.24 %, Temperature 120 °C |
1190 psi @Strain 157.24 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.20 MPa @Strain 50.0 %, Temperature 23.0 °C |
1190 psi @Strain 50.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |