Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.20 MPa @Strain 300 % |
1190 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4885 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 8.22 MPa @Strain 0.150 %, Temperature 90.0 °C |
1190 psi @Strain 0.150 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Stress | 8.20 MPa @Strain 1.10 %, Temperature 90.0 °C |
1190 psi @Strain 1.10 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 8.21 MPa @Strain 0.700 %, Temperature 100 °C |
1190 psi @Strain 0.700 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 8.21 MPa @Strain 44.65 %, Temperature 100 °C |
1190 psi @Strain 44.65 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.19 MPa @Strain 100.7 %, Temperature 120 °C |
1190 psi @Strain 100.7 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.21 MPa @Strain 3.83 %, Temperature 90.0 °C |
1190 psi @Strain 3.83 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.21 MPa @Strain 184.09 %, Temperature 120 °C |
1190 psi @Strain 184.09 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.18 MPa @Strain 0.200 %, Temperature 160 °C |
1190 psi @Strain 0.200 %, Temperature 320 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
Tensile Stress | 8.19 MPa @Strain 19.46 %, Temperature 90.0 °C |
1190 psi @Strain 19.46 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 8.21 MPa @Strain 145.5 %, Temperature 160 °C |
1190 psi @Strain 145.5 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 8.20 MPa @Strain 15.0 %, Temperature 23.0 °C |
1190 psi @Strain 15.0 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
Tensile Stress | 8.20 MPa @Strain 157.24 %, Temperature 120 °C |
1190 psi @Strain 157.24 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.20 MPa @Strain 50.0 %, Temperature 23.0 °C |
1190 psi @Strain 50.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Tensile Stress | 8.19 MPa @Strain 19.46 %, Temperature 90.0 °C |
1190 psi @Strain 19.46 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.21 MPa @Strain 145.5 %, Temperature 160 °C |
1190 psi @Strain 145.5 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |