Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 96.7 MPa @Strain 11.1 %, Temperature -40.0 °C |
14000 psi @Strain 11.1 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |
|||
Tensile Stress | 96.7 MPa @Strain 0.990 %, Temperature 23.0 °C |
14000 psi @Strain 0.990 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |