Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 6.90 - 8.60 MPa | 1000 - 1250 psi | ASTM D790 |
Multibase Multi-Flex® TPE D 4107 This product is UV stabilized for automotive applications, like fender guards and airbags. The Xenon Arc is 2.5 Delta E, ASTM SAE J1960 1240 KJ/m². Passes Impact resistance test ASTM GM 9032 P at.. |
|||
Flexural Strength | 6.90 - 8.60 MPa | 1000 - 1250 psi | ASTM D790-95 |
Multibase Multi-Flex® TPO 1047-4107 Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags.Data provided by Multibase. |
|||
Flexural Strength | 6.89 MPa | 1000 psi | ASTM D790 |
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Flexural Strength | 6.90 - 10.3 MPa | 1000 - 1490 psi | |
Ceradyne Thermo-Sil® Castable TG Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |