Material Notes:
Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792-91
Melt Flow 8.0 g/10 min
8.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 42
42
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 10.3 - 14.5 MPa
1490 - 2100 psi
ASTM D638-95
Elongation at Break 500 - 700 %
500 - 700 %
ASTM D638-95
Flexural Strength 6.90 - 8.60 MPa
1000 - 1250 psi
ASTM D790-95
Flexural Modulus 0.213 - 0.255 GPa
30.9 - 37.0 ksi
Secant 1%; ASTM D-790-95
Tear Strength Test 65 - 88
65 - 88
ASTM D624-95
Optical Properties Metric English Comments
Gloss 38 %
38 %
ASTM D2457-90