Polymer Property : Flexural Strength = 1250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 6.90 - 8.60 MPa
1000 - 1250 psi
ASTM D790
Multibase Multi-Flex® TPE D 4107
This product is UV stabilized for automotive applications, like fender guards and airbags. The Xenon Arc is 2.5 Delta E, ASTM SAE J1960 1240 KJ/m². Passes Impact resistance test ASTM GM 9032 P at..
Flexural Strength 6.90 - 8.60 MPa
1000 - 1250 psi
ASTM D790-95
Multibase Multi-Flex® TPO 1047-4107
Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags.Data provided by Multibase.