Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.98 MPa | 12470 psi | ASTM D790 |
Aclo Accutech ABS ABS832G10L Glass Reinforced |
|||
Flexural Strength | 85.98 MPa | 12470 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336G20M10CL Glass/Mineral Reinforced Coupled |