Polymer Property : Flexural Strength = 85.98 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 85.98 MPa
12470 psi
ASTM D790
Aclo Accutech ABS ABS832G10L Glass Reinforced
Flexural Strength 85.98 MPa
12470 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0336G20M10CL Glass/Mineral Reinforced Coupled