Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 124 - 138 MPa | 18000 - 20000 psi | ASTM D790 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | ASTM D790 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu.. |
|||
Flexural Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl.. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab.. |
|||
Flexural Strength | 96.5 - 138 MPa | 14000 - 20000 psi | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Flexural Strength | 117 - 138 MPa | 17000 - 20000 psi | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext.. |
|||
Flexural Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Flexural Strength | 96.5 - 138 MPa | 14000 - 20000 psi | |
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, .. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better .. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Flexural Strength | 96.5 - 138 MPa | 14000 - 20000 psi | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in .. |
|||
Flexural Strength | 110 - 138 MPa | 16000 - 20000 psi | |
Bulk Molding Compounds BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, medi.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 6605A Polyester Molding Compound |
|||
Flexural Strength | 117 - 138 MPa | 17000 - 20000 psi | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Flexural Strength | 124 - 138 MPa | 18000 - 20000 psi | |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |