Polymer Property : Flexural Strength = 152 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 131 - 152 MPa
19000 - 22000 psi
ASTM D790
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Flexural Strength 131 - 152 MPa
19000 - 22000 psi
ASTM D790
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Flexural Strength 68.9 - 152 MPa
10000 - 22000 psi
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound
BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati..
Flexural Strength 124 - 152 MPa
18000 - 22000 psi
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound
BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers.
Flexural Strength 124 - 152 MPa
18000 - 22000 psi
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound
BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic..
Flexural Strength 124 - 152 MPa
18000 - 22000 psi
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound
BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o..