Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 11.0 MPa | 1600 psi | |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP R1000S PA 66 LNP COLORCOMP* R1000S is an unfilled Nylon 66. Added features of this material is: Heat Stabilized. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP R1000SU PA 66 LNP COLORCOMP* R1000SU is an unfilled Nylon 66 resin. Added features include: Heat Stabilized, UV Stabilized. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | ASTM D790M |
DSM Somos® 8110 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Flexural Strength | >= 11.0 MPa | >= 1600 psi | |
MarkeTech Repton 601 Mullite Brand 601 features: High porosity-low bulk density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e.. |
|||
Flexural Strength | >= 11.0 MPa | >= 1600 psi | |
MarkeTech Repton EXP 338 Alumina 99.6% EXP 338 features high porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cyc.. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | |
UCAR Carbon UCAR® PGX Pressure Molded Graphite Available in low ash monolithic sizes as large as 73" diameter, Grade PGX has excellent erosion resistance and thermal properties.Typical Applications:Fluidized bed reactors Centrifugal casting mold.. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | Olsen; ASTM D747 |
UBE J5019 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | ASTM D790 |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | SAE J949 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Strength | 11.0 MPa | 1600 psi | SAE J949 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |