Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Somos® 8110 Epoxy Photopolymer  (discontinued **)

Category Polymer , Rapid Prototyping Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Somos® 8110 Epoxy Photopolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and excellent tolerance to a wide temperature and humidity range during and after build. This material is especially useful in functional applications where flexibility and impact-strength are critical requirements (e.g. plastic bottles, packaging, automobile panels, electronic enclosures, medical products, and snap-fit parts).ApplicationSomos® 8110 Photopolymer is used in the solid imaging process to build three-dimensional parts.Information Provided by DSM Desotech Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc

@Temperature 25.0 °C
0.0401 lb/in³

@Temperature 77.0 °F
Viscosity 600 cP

@Temperature 30.0 °C
600 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
ASTM D2240
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638M
Elongation at Break 27 %
27 %
ASTM D638M
Modulus of Elasticity 0.317 GPa
46.0 ksi
ASTM D638M
Flexural Strength 11.0 MPa
1600 psi
ASTM D790M
Flexural Modulus 0.310 GPa
45.0 ksi
ASTM D790M
Izod Impact, Notched 0.870 J/cm
1.63 ft-lb/in
ASTM D256A
Tear Strength, Total 196 N
44.1 lb (f)
Graves; ASTM D1004
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °C
129 °F
ASTM D648
Descriptive Properties Value Comments
Appearance Transparent Amber
Dp (mm) 0.135
Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2) 40
Exposure that gives 0.254mm thickness
E5 (mJ/cm2) 15
Exposure that gives 0.127mm thickness
Ec (mJ/cm2) 6
Critical exposure
Users viewing this material also viewed the following: