Polymer Property : Flexural Strength = 243 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength <= 243 MPa
<= 35200 psi
ISO 178
Polykemi AB SCANAMID 66.6 C12^F30 Nylon 66/6, Glass Fiber, Reinforced
Information provided by Polykemi AB
Flexural Strength 243 MPa
35200 psi
ISO 178
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized..
Flexural Strength 243 MPa
35200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK
LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber.
Flexural Strength 243 MPa
35200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific)
LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Flexural Strength 243 MPa
35200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
Flexural Strength 243 MPa
35200 psi
2 mm/min; ISO 178
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber
SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers
Flexural Strength 243 MPa
35200 psi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6
LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Strength 243 MPa
35200 psi
DAM; ISO 178
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr..