Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 25100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 173 MPa
25100 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC
LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
Flexural Strength 173 MPa

@Temperature 100 °C
25100 psi

@Temperature 212 °F
ISO 178
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Flexural Strength 173 MPa

@Temperature 150 °C
25100 psi

@Temperature 302 °F
ASTM D790
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Strength 173 MPa
25100 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66
LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding.
Flexural Strength 173 MPa
25100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT
LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
Flexural Strength 173 MPa
25100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66
LNP LUBRILOY* RF206 is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material includes: Wear Resistant.
Flexural Strength 173 MPa
25100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRILOY RF206AXH PA 66
LNP LUBRILOY* RF206AXH is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material include: Wear Resistant, Healthcare.
Flexural Strength 173 MPa
25100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC
LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive.
Flexural Strength 173 MPa
25100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® K4560 PBT
30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable.
Flexural Strength 173 MPa
25100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East)
30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable.
Flexural Strength 173 MPa
25100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RX06001 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RX06001 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Easy Molding, High Impact, Electrically Conductive.
Flexural Strength 173 MPa
25100 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12
LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber.
Flexural Strength 173 MPa
25100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66
LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare.
Flexural Strength 173 MPa
25100 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT
LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact.
Flexural Strength 173 MPa
25100 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT
LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber.
Flexural Strength 173 MPa
25100 psi
ISO 178
Polyplastics Duranex® 3216 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Strength 173 MPa
25100 psi
ISO 178
Azoty Tarnow™ TARNOFORM 300 GF5 POM
26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Flexural Strength 173 MPa
25100 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific)
LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.
Flexural Strength 173 MPa
25100 psi
ASTM D 790
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP
LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg..
Copyright © lookpolymers.com All Rights Reserved