Polymer Property : Flexural Strength = 30300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 209 MPa
30300 psi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6
LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..
Flexural Strength 209 MPa
30300 psi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Flexural Strength 209 MPa
30300 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific)
Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN..
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES
LNP* THERMOCOMP* JF006E is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK
LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber.
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific)
LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific)
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66
LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead.
Flexural Strength 209 MPa
30300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON MV00AS PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, heat stabilized
Flexural Strength 209 MPa
30300 psi
GB/9341
Zhejiang Juner PA66-301-HG30 Flame-Retardant & Glass Reinforced, Environmental PA66
Applications: Connector AS PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Flexural Strength 209 MPa

@Temperature 23.0 °C
30300 psi

@Temperature 73.4 °F
EN ISO 178
Ensinger TECASINT 1101 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East)
LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Strength 209 MPa
30300 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF006EXZ PES
LNP* THERMOCOMP* JF006EXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.