Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner PA66-301-HG30 Flame-Retardant & Glass Reinforced, Environmental PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PA66-301-HG30 Flame-Retardant & Glass Reinforced, Environmental PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Connector AS PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
GB/1033
Water Absorption 0.60 %
0.60 %
23°C•24h
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
GB/15585
Mechanical Properties Metric English Comments
Tensile Strength, Yield 137 MPa
19900 psi
GB/1040
Flexural Strength 209 MPa
30300 psi
GB/9341
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
IS0179-1:2000
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
GB1634
Flammability, UL94 V-0
V-0
GB/T2408
Flammability Test 30
30
Flame Remainder (%); GB/9345
Processing Properties Metric English Comments
Processing Temperature 255 - 285 °C
491 - 545 °F
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Drying Temperature 110 °C

@Time 10800 sec
230 °F

@Time 3.00 hour
Vacuum Pressure, -0.08 MPa
120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
Chute Hot-Wind
120 °C

@Time 21600 sec
248 °F

@Time 6.00 hour
Horizontal Oven
Injection Pressure 50.0 - 120 MPa
7250 - 17400 psi
Descriptive Properties Value Comments
Speed of Shoot, % 35-90
Users viewing this material also viewed the following: