Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 314 MPa @Temperature 150 °C |
45500 psi @Temperature 302 °F |
ASTM D790 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Crystalline
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Strength | 314 MPa | 45600 psi | ASTM D790 |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Strength | 314 MPa | 45600 psi | ASTM D790 |
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Strength | 314 MPa | 45500 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Flexural Strength | 314 MPa | 45500 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Flexural Strength | 314 MPa @Temperature 23.0 °C |
45500 psi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers VESPEL TP-8130 Polyimide DuPont Vespel TP-8130 parts are specified for mechanical, thermal, and tribological properties. TP-8130 parts exhibits excellent strength and toughness, dimensional stability, low outgassing, radiat.. |
|||
Flexural Strength | 314 MPa | 45500 psi | Dry; ASTM D790 |
Asahi Kasei Leona® 13G43 43% Glass Filled Nylon 66 43% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Mechanical and electrical parts such as micromotors, automotive parts such as radiator tanks and shift leversInformation provi.. |