Polymer Property : Flexural Strength = 317 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 317 MPa
46000 psi
ASTM D790
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Strength 317 MPa
46000 psi
ASTM D790
PolyOne Edgetek® NN-50GF/000EM L Polyamide 66 (Nylon 66)
Information provided by PolyOne
Flexural Strength 317 MPa
46000 psi
ASTM D790
PolyOne Nymax™ GF 1200 A 55 HS Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Flexural Strength 317 MPa
46000 psi
ASTM D790
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Flexural Strength 317 MPa
46000 psi
ASTM D-790
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas..
Flexural Strength 317 MPa
46000 psi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope..
Flexural Strength 317 MPa
46000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP LCL36E PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LCL36E is a compound based on Polyetheretherketone resin containing Carbon Fiber , PTFE. Added features include : Electrically Conductive, Internally Lubricated, Easy Molding.
Flexural Strength 317 MPa
46000 psi
ASTM D790
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Flexural Strength 317 MPa
46000 psi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..
Flexural Strength 317 MPa
46000 psi
ASTM D790
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat..
Flexural Strength 317 MPa
46000 psi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66
LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b..
Flexural Strength 317 MPa
46000 psi
ASTM D790
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Flexural Strength 317 MPa
46000 psi
ASTM D790
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T..
Flexural Strength 317 MPa
46000 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RX89047 PA 66
LNP* VERTON* RX89047 is a compound based on Nylon 66 resin containing Proprietary Fillers. Added feature of this grade is: Structural.
Flexural Strength 317 MPa
46000 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Asia Pacific)
LNP* Verton* RX89047 is a compound based on Nylon 66 resin.
Flexural Strength 317 MPa
46000 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Europe-Africa-Middle East)
LNP* Verton* RX89047 is a compound based on Nylon 66 resin.
Flexural Strength 317 MPa
46000 psi
2 mm/min; ISO 178
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber
SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers
Flexural Strength 317 MPa
46000 psi
ASTM D790
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Flexural Strength 317 MPa
46000 psi
ASTM D790
Chase Plastics CP Pryme® NN143GL (DAM) Nylon 66, 43% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 317 MPa
46000 psi
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina
Parts fabricated to print. Excellent physical properties and corrosion resistance. For pump liners, nozzles, guides. Standard crucibles and bolts, nuts and washers from 4-40 to 1/4-20.
Flexural Strength 317 MPa
46000 psi
ASTM D790
PolyOne Edgetek® NL-30CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.
Flexural Strength 317 MPa
46000 psi
ASTM D790
Techmer ES HiFill FR® PA6/6 GF50 FR UV X BK 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightAdditive: Flame Retardant and UV StabilizerFeatures: Flame RetardantAppearance: BlackProcessing Method..