Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer Lubrizol (former Noveon)
Trade Name Isoplast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Tensile Strength, Yield 179 MPa
26000 psi
ASTM D638
Elongation at Break 1.6 %
1.6 %
ASTM D638
Elongation at Yield 1.6 %
1.6 %
ASTM D638
Tensile Modulus 16.0 GPa
2320 ksi
ASTM D638
Flexural Strength 317 MPa
46000 psi
ASTM D790
Flexural Modulus 14.0 GPa
2030 ksi
ASTM D790
Izod Impact, Unnotched 6.41 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
12.0 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 °C
6.11 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
Unannealed; ASTM D648
127 °C
261 °F
Annealed; ASTM D648
Vicat Softening Point 186 °C
367 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 65.0 - 90.0 °C
149 - 194 °F
Drying Temperature 80.0 - 100 °C
176 - 212 °F