Mechanical Properties Metric English Comments
Flexural Strength 37.2 MPa
5400 psi
ASTM D790-95
Multibase Multi-Pro® 0110 X Natural Polypropylene
This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide..
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
PolyOne Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Strength 37.2 MPa
5400 psi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers SBS 1000 Clear Styrene Butadiene Copolymer
Description: Clear Styrene Butadiene CopolymerInformation provided by Network Polymers Inc.
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
PolyOne Maxxam™ FR PP 301 EXT Polypropylene, Unspecified (PP, Unspecified)
Information provided by PolyOne
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled  (discontinued **)<
Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Flexural Strength 37.2 MPa
5400 psi
ASTM D 790
Styrolution Clearblend 165 MBS
CLEARBLEND 165 is an impact modified styrene acrylic copolymer blend with excellent clarity and outstanding toughness.Exceptional toughnessLow densityEase of processingLow moisture absorptionInforma..
Flexural Strength 37.2 MPa

@Thickness 3.20 mm
5400 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 556 Flame Retardant Polystyrene
Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect..
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Chase Plastics CP Pryme® NN300HSL (COND, 50% RH) Nylon 66 (Utility Grade), Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Chase Plastics CP Pryme® NN300L (COND, 50% RH) Nylon 66 (Utility Grade), Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 37.2 MPa
5400 psi
chs 0.05 in/min; ASTM D790
Diamond Polymers SBS 1031 Clear Styrene Butadiene Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene
Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa..
Flexural Strength 37.2 MPa
5400 psi
Anderman Ceramics EM60P Sillimanite
Porous synthetic mullite with high thermal shock. Available as tube up to 10 ft (3 m) long with diameters 0.6" to 2.4".Information provided by Anderman Ceramics.
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Adell EZ-18 Homopolymer Polypropylene, 40% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled
Data provided by Adell Plastics, Inc.