Mechanical Properties Metric English Comments
Flexural Strength 379 MPa
55000 psi
Pyrotek TS-207 Thermoset Electrical Insulation Product
Polymer reinforcement, Polyester resin, Grey color. High strength and good electrical resistance.Information provided by Pyrotek.
Flexural Strength 379 MPa
55000 psi
ASTM D790
PolyOne Edgetek® NN-40CF/000 - OBSOLETE Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Strength 379 MPa
55000 psi
ASTM D-790
PlastiComp Complet® LCF30 - PA6 Nylon 6, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Flexural Strength 379 MPa
55000 psi
MTI ThermoStran® PA66-30C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Flexural Strength 379 MPa
55000 psi
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Flexural Strength 379 MPa

@Strain 3.50 %
55000 psi

@Strain 3.50 %
ISO 178
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface ..
Flexural Strength 379 MPa
55000 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA (Asia Pacific)
LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 379 MPa
55000 psi
ASTM D790
Techmer ES HiFill® HDPE TM20 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Strength 379 MPa
55000 psi
ASTM D790
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi..
Flexural Strength 379 MPa
55000 psi
ASTM D790
Techmer ES HiFill® HDPE TM25 25% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Strength 379 MPa
55000 psi
ASTM F417
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Flexural Strength 379 MPa
55000 psi
MOR; ASTM-F417
CoorsTek AD-996 99.6% Alumina
Flexural Strength 379 MPa
55000 psi
MOR; ASTM-F417
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..