Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 4005 MPa | 580900 psi | 1190°C Hardening Temperature, 550°C Tempering Temperature; 67 Rockwell Hardness C |
Crucible Compaction Metals CPM® VIM CRU® 20® CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle.. |
|||
Flexural Strength | 4005 MPa | 580900 psi | Hardening Temperature- 1190°C, Tempering Temperature- 550°C |
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea.. |
|||
Flexural Strength | 4005 MPa | 580900 psi | Hardening Temperature- 1235°C, Tempering Temperature- 540°C |
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS) CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobal.. |