Polymer Property : Flexural Strength = 580900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 4005 MPa
580900 psi
1190°C Hardening Temperature, 550°C Tempering Temperature; 67 Rockwell Hardness C
Crucible Compaction Metals CPM® VIM CRU® 20®
CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle..
Flexural Strength 4005 MPa
580900 psi
Hardening Temperature- 1190°C, Tempering Temperature- 550°C
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel
CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea..
Flexural Strength 4005 MPa
580900 psi
Hardening Temperature- 1235°C, Tempering Temperature- 540°C
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS)
CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobal..