Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 52.0 MPa | 7540 psi | |
Ohio Carbon Blank OCB AR-12 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nemcon™ H ABS DP116P ABS ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Flexural Strength | <= 52.0 MPa | <= 7540 psi | ISO 178 |
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 52.0 MPa | <= 7540 psi | ISO 178 |
Polykemi AB POLYfill PPH K20020 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | <= 52.0 MPa | <= 7540 psi | ISO 178 |
Polykemi AB POLYfill PPH K20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification.. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 850 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Custom colorsApplications: Injection molding or extrusion, Suitable replacement for some engineering resins, Toys, Packaging, Business eq.. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
Stratasys® ABSplus ABSplus is up to 40 percent stronger than standard ABS material and is an ideal material for conceptual prototyping through design verification through direct digital manufacturing. The marriage of .. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0150AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | At Rupture; ASTM D790 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | At Rupture; ASTM D790 |
Sumitomo Bakelite North America SI 9045C Silicone Compound Long fiberglass and graphite filled silicone molding compound which offers moderate strength properties, high impact resistance, and excellent thermal stability at elevated temperatures.Information .. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
Teknor Apex Sinpolene TPP1020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 20% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
Teknor Apex Sinpolene TPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 40% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ISO 178 |
Unitika A3030N-2 PA6, 30% Mineral Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Flexural Strength | 52.0 - 71.0 MPa | 7540 - 10300 psi | ASTM D790 |
3D Systems Accura® Xtreme Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte.. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437G20M10CL Glass/Mineral Reinforced Coupled |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334G10CL Glass Reinforced Coupled |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ISO 178 |
Cathay PA514 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
3M Scotchkote™ 162HB Epoxy Coating 3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw w.. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 608 Nylon 6/12, Impact Modified Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 CI2 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 10% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Flexural Strength | 52.0 MPa | 7540 psi | At Rupture; ASTM D790 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |