Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 4.00 - 82.7 MPa | 580 - 12000 psi | Average value: 14.5 MPa Grade Count:56 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Compressive Yield Strength | 57.9 - 82.7 MPa | 8400 - 12000 psi | Average value: 71.7 MPa Grade Count:7 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |