Polymer Property : Compressive Yield Strength = 82.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 4.00 - 82.7 MPa
580 - 12000 psi
Average value: 14.5 MPa Grade Count:56
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Compressive Yield Strength 57.9 - 82.7 MPa
8400 - 12000 psi
Average value: 71.7 MPa Grade Count:7
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..