Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 150.4 MPa | 21810 psi | ASTM D695 |
Plenco 50015 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |