Mechanical Properties Metric English Comments
Compressive Yield Strength 150.4 MPa
21810 psi
ASTM D695
Plenco 50015 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu..