Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 48.3 - 170 MPa | 7000 - 24700 psi | Average value: 71.2 MPa Grade Count:7 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |