Mechanical Properties Metric English Comments
Compressive Yield Strength 48.3 MPa
7000 psi
Mixed 1:1; TM R050-38
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Compressive Yield Strength 48.3 - 58.6 MPa
7000 - 8500 psi
Average value: 53.4 MPa Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Compressive Yield Strength 48.3 MPa
7000 psi
TM R050-38
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to..
Compressive Yield Strength 48.3 MPa
7000 psi
TM R050-38
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to..
Compressive Yield Strength 48.3 - 170 MPa
7000 - 24700 psi
Average value: 71.2 MPa Grade Count:7
Overview of materials for Polypropylene with 20% Glass Fiber Filler