Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.970 - 1.46 g/cc
0.0350 - 0.0527 lb/in³
Average value: 1.06 g/cc Grade Count:237
Filler Content 15.0 - 23.0 %
15.0 - 23.0 %
Average value: 19.1 % Grade Count:97
Water Absorption 0.0100 - 0.0500 %
0.0100 - 0.0500 %
Average value: 0.0197 % Grade Count:40
Additive Loading 20.0 %
20.0 %
Average value: 20.0 % Grade Count:5
Maximum Moisture Content 0.0100
0.0100
Average value: 0.0100 Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0320 cm/cm
0.00100 - 0.0320 in/in
Average value: 0.00502 cm/cm Grade Count:190
Linear Mold Shrinkage, Transverse 0.00400 - 0.0206 cm/cm
0.00400 - 0.0206 in/in
Average value: 0.0109 cm/cm Grade Count:17
Melt Flow 0.500 - 34.0 g/10 min
0.500 - 34.0 g/10 min
Average value: 7.61 g/10 min Grade Count:164
Ash 13.0 - 23.0 %
13.0 - 23.0 %
Average value: 19.5 % Grade Count:11
Mechanical Properties Metric English Comments
Hardness, Rockwell M 53.0 - 105
53.0 - 105
Average value: 67.2 Grade Count:5
Hardness, Rockwell R 80.0 - 115
80.0 - 115
Average value: 96.6 Grade Count:56
Hardness, Shore D 70.0 - 75.0
70.0 - 75.0
Average value: 73.6 Grade Count:25
Tensile Strength, Ultimate 22.0 - 115 MPa
3190 - 16700 psi
Average value: 60.9 MPa Grade Count:150
9.00 - 60.0 MPa

@Temperature 60.0 - 120 °C
1310 - 8700 psi

@Temperature 140 - 248 °F
Average value: 36.3 MPa Grade Count:4
Tensile Strength, Yield 25.0 - 90.0 MPa
3630 - 13100 psi
Average value: 59.6 MPa Grade Count:99
Elongation at Break 1.00 - 100 %
1.00 - 100 %
Average value: 5.65 % Grade Count:170
2.40 - 2.60 %

@Temperature 80.0 - 80.0 °C
2.40 - 2.60 %

@Temperature 176 - 176 °F
Average value: 2.50 % Grade Count:3
Elongation at Yield 2.00 - 11.0 %
2.00 - 11.0 %
Average value: 4.43 % Grade Count:51
Modulus of Elasticity 1.03 - 6.55 GPa
149 - 950 ksi
Average value: 4.22 GPa Grade Count:97
3.30 - 3.40 GPa

@Temperature 80.0 - 80.0 °C
479 - 493 ksi

@Temperature 176 - 176 °F
Average value: 3.37 GPa Grade Count:3
Flexural Yield Strength 32.0 - 170 MPa
4640 - 24700 psi
Average value: 86.9 MPa Grade Count:184
82.0 - 90.0 MPa

@Temperature 80.0 - 80.0 °C
11900 - 13100 psi

@Temperature 176 - 176 °F
Average value: 87.3 MPa Grade Count:3
Flexural Modulus 1.49 - 6.76 GPa
217 - 980 ksi
Average value: 3.53 GPa Grade Count:240
0.800 - 3.40 GPa

@Temperature 60.0 - 120 °C
116 - 493 ksi

@Temperature 140 - 248 °F
Average value: 2.45 GPa Grade Count:4
Compressive Yield Strength 48.3 - 170 MPa
7000 - 24700 psi
Average value: 71.2 MPa Grade Count:7
Izod Impact, Notched 0.135 - 4.50 J/cm
0.253 - 8.43 ft-lb/in
Average value: 0.940 J/cm Grade Count:178
0.350 - 0.800 J/cm

@Temperature -40.0 - 0.000 °C
0.656 - 1.50 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.533 J/cm Grade Count:4
0.5339 - 0.5339 J/cm

@Temperature -28.9 - -28.9 °C
1.000 - 1.000 ft-lb/in

@Temperature -20.0 - -20.0 °F
Average value: 0.533 J/cm Grade Count:1
0.5339 - 0.5339 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 1.000 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.533 J/cm Grade Count:1
Izod Impact, Unnotched 0.747 - 8.54 J/cm
1.40 - 16.0 ft-lb/in
Average value: 4.35 J/cm Grade Count:79
Izod Impact, Notched (ISO) 4.00 - 38.0 kJ/m²
1.90 - 18.1 ft-lb/in²
Average value: 13.3 kJ/m² Grade Count:18
2.00 - 10.0 kJ/m²

@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 7.11 kJ/m² Grade Count:9
Izod Impact, Unnotched (ISO) 27.0 - 65.0 kJ/m²
12.8 - 30.9 ft-lb/in²
Average value: 39.0 kJ/m² Grade Count:8
13.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
6.19 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 27.3 kJ/m² Grade Count:6
Charpy Impact Unnotched 2.30 - 7.00 J/cm²
10.9 - 33.3 ft-lb/in²
Average value: 4.49 J/cm² Grade Count:27
1.10 - 6.00 J/cm²

@Temperature -40.0 - -20.0 °C
5.24 - 28.6 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.55 J/cm² Grade Count:25
Charpy Impact, Notched 0.200 - 2.70 J/cm²
0.952 - 12.8 ft-lb/in²
Average value: 1.11 J/cm² Grade Count:55
0.100 - 2.00 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 9.52 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.596 J/cm² Grade Count:39
Gardner Impact 0.282 - 2.09 J
0.208 - 1.54 ft-lb
Average value: 0.746 J Grade Count:41
Thermal Properties Metric English Comments
CTE, linear 4.32 - 80.0 µm/m-°C
2.40 - 44.4 µin/in-°F
Average value: 41.8 µm/m-°C Grade Count:33
Thermal Conductivity 0.288 - 1.21 W/m-K
2.00 - 8.40 BTU-in/hr-ft²-°F
Average value: 0.442 W/m-K Grade Count:6
Melting Point 130 - 182 °C
266 - 360 °F
Average value: 162 °C Grade Count:30
Maximum Service Temperature, Air 65.0 - 180 °C
149 - 356 °F
Average value: 115 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 96.1 - 205 °C
205 - 401 °F
Average value: 149 °C Grade Count:153
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 190 °C
140 - 374 °F
Average value: 131 °C Grade Count:211
Vicat Softening Point 79.0 - 205 °C
174 - 401 °F
Average value: 126 °C Grade Count:44
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:102
Electrical Properties Metric English Comments
Electrical Resistivity 1000 - 4.00e+16 ohm-cm
1000 - 4.00e+16 ohm-cm
Average value: 1.25e+16 ohm-cm Grade Count:37
Surface Resistance 1e+05 - 1.00e+15 ohm
1e+05 - 1.00e+15 ohm
Average value: 5.13e+14 ohm Grade Count:8
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:3
Dielectric Constant 2.60 - 3.00
2.60 - 3.00
Average value: 2.75 Grade Count:12
Dielectric Strength 17.3 - 22.0 kV/mm
440 - 559 kV/in
Average value: 20.6 kV/mm Grade Count:21
Dissipation Factor 0.00100 - 0.00200
0.00100 - 0.00200
Average value: 0.00109 Grade Count:11
Arc Resistance 80.0 - 130 sec
80.0 - 130 sec
Average value: 119 sec Grade Count:9