Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 33100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 228 MPa
33100 psi
ASTM D695
Plenco 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound  (discontinued **)
Plaslok 201 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to have an excellent balance of molded properties. The material provides good electrical insulation val..
Compressive Yield Strength 228 MPa
33100 psi
ASTM D695
Plenco 7021 Black Impact Grade Phenolic Molding Compound  (discontinued **)
Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of..
Compressive Yield Strength 228 MPa
33100 psi
ASTM D695
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min..
Compressive Yield Strength 228 MPa
33100 psi
ASTM D695
Plaslok 7021 Black Impact Grade Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7021 is the replacement material for ..