Polymer Property : Compressive Yield Strength = 37100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 55.2 - 256 MPa
8000 - 37100 psi
Average value: 169 MPa Grade Count:8
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..