Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 55.2 - 256 MPa | 8000 - 37100 psi | Average value: 169 MPa Grade Count:8 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Compressive Yield Strength | 55.2 MPa | 8000 psi | ASTM D695 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Compressive Yield Strength | 55.2 MPa | 8000 psi | ASTM D695 |
Westlake Plastics Propylux® HS Polypropylene-heat stabilized For Medical Applications Medical grade Propylux HS is made from an FDA approved polypropylene resin. Through a unique heat-stabilizing process, the extruded material is able to withstand higher temperature with less water .. |