Polymer Property : Compressive Modulus = 2.07 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.38 - 2.07 GPa
200 - 300 ksi
ASTM D695
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon
Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau..
Compressive Modulus 0.847 - 2.07 GPa
123 - 300 ksi
Average value: 1.55 GPa Grade Count:11
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..