Polymer Property : Compressive Modulus = 0.847 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.847 - 112 GPa
123 - 16200 ksi
Average value: 6.87 GPa Grade Count:29
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Compressive Modulus 0.847 GPa

@Temperature 23.0 °C
123 ksi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Modulus 0.847 - 2.07 GPa
123 - 300 ksi
Average value: 1.55 GPa Grade Count:11
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..