Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.847 - 112 GPa | 123 - 16200 ksi | Average value: 6.87 GPa Grade Count:29 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Compressive Modulus | 0.850 GPa | 123 ksi | Loading, In the In Plane Direction |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Compressive Modulus | 0.847 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Compressive Modulus | 0.847 - 2.07 GPa | 123 - 300 ksi | Average value: 1.55 GPa Grade Count:11 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |