Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.34 GPa | 340 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/4-5052-.004 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 2.34 GPa | 339 ksi | |
Trelleborg AEM Syntac® 350 Syntactic Foam Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro.. |
|||
Compressive Modulus | 2.34 GPa | 339 ksi | |
Trelleborg AEM Syntac® 351 Syntactic Foam Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli.. |
|||
Compressive Modulus | 2.34 GPa | 340 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 2.34 GPa | 340 ksi | ASTM D695 |
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Compressive Modulus | 2.34 GPa | 340 ksi | TM R050-38 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |