Trelleborg AEM Syntac® 350 Syntactic Foam

Category Polymer , Thermoset , Epoxy
Manufacturer Trelleborg AEM
Trade Name Syntac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg AEM Syntac® 350 Syntactic Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and rod form, Syntac® 350 is easily machined using standard shop tools and offers a lightweight, durable and cost effective alternative to wood, felt and aluminumAll information provided by Trelleborg Emerson & Cuming
Physical Properties Metric English Comments
Density 0.673 g/cc
0.0243 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 55

@Temperature 177 °C
55

@Temperature 350 °F
Compressive Strength 44.8 MPa
6500 psi
Compressive Modulus 2.34 GPa
339 ksi
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C
17.0 µin/in-°F
Specific Heat Capacity 2.09 J/g-°C
0.500 BTU/lb-°F
Thermal Conductivity 0.121 W/m-K
0.840 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: